[MKNANO] Absorption: 490 nm, Emission: 530 nm, Size: 3.7 nm
Product
Absorption: 490 nm, Emission: 530 nm, Size: 3.7 nm
Product Number
MKN-InP/ZnS-T530
CAS Number
Formula
InP/ZnS
Product Details
InP/ZnS Core-Shell Nanocrystals in Toluene
stabilized by oleylamine ligands
Organic Impurities: 1% (not including ligands)
PL fwhm (nm): 58-70
UV-Vis hwhm (nm): 34-46
Absorption: 490 nm, Emission: 530 nm, Size: 3.7 nm
Quantum Yield: ~30%
This product can also offered in Hexanes or Chloroform or Dichloromethane or Methanol
stabilized by oleylamine ligands
Organic Impurities: 1% (not including ligands)
PL fwhm (nm): 58-70
UV-Vis hwhm (nm): 34-46
Absorption: 490 nm, Emission: 530 nm, Size: 3.7 nm
Quantum Yield: ~30%
This product can also offered in Hexanes or Chloroform or Dichloromethane or Methanol
'MKNANO' 카테고리의 다른 글
[MKNano] Emission Peak: 570 nm (0) | 2023.04.06 |
---|---|
[Mknano] Nickel Oxide NanoWires (0) | 2023.01.31 |
[MKNANO] Short Length, Pure, OD: 2-4 nm (0) | 2022.06.21 |
[MKNANO] CdS in Hexanes, Chloroform, Dichloromethane, Methanol (0) | 2022.02.22 |
[MKNANO] Magnetic Iron Oxide Nanocrystals in non-polar Solvent (0) | 2022.02.15 |